Back to News list

What is CO2 welding and how does it work in industrial applications

2026-11-28

What is CO2 welding and how does it work in industrial applications

Article overview

This article explains what CO2 welding is, how it functions as part of the gas metal arc welding (GMAW) process, and why it is widely used across Indonesian industrial sectors. It covers the core mechanics, parameter setup, common problems such as spatter and porosity, comparisons with mixed-gas and flux core alternatives, and practical guidance for workshop and fabrication environments.

CO2 welding is a form of gas metal arc welding (GMAW) that uses carbon dioxide as the shielding gas to protect the weld pool from atmospheric contamination. It feeds a continuous solid wire electrode through a welding gun, creates an arc between the wire and the base metal, and melts both together to form a weld joint. In Indonesia, the process is commonly called las CO2 and represents the dominant MIG/MAG welding method used in workshops, fabrication yards, and manufacturing lines — not because it is a simplified alternative, but because it is cost-effective, fast, and entirely capable of producing structural-quality welds on carbon steel and low-alloy steel when set up correctly.

What CO2 welding actually is — and why the terminology matters

The confusion around terminology is worth addressing directly. "CO2 welding," "MIG welding," "MAG welding," and "GMAW" all describe related processes, and they are frequently used interchangeably on the shop floor — sometimes accurately, sometimes not.

GMAW (gas metal arc welding) is the umbrella term for any arc welding process that uses a continuously fed wire electrode and a shielding gas. Under that umbrella, two variants matter most:

  • MIG (metal inert gas welding) — uses a truly inert gas, such as pure argon. This is correct for welding aluminum and other non-ferrous metals where any oxidizing reaction would damage the weld.
  • MAG (metal active gas welding) — uses an active gas, either pure CO2 or a mixture of argon and CO2. This is what happens in virtually all carbon steel welding, including what is called "las CO2" in Indonesian workshops.

So technically, CO2 welding is a MAG process, not MIG. However, the term "MIG welding" has become so widely used as a shorthand for wire feed welding in general that most welders, suppliers, and even equipment catalogs use MIG and MAG interchangeably when talking about steel. For the purposes of this article, co2 welding refers specifically to the MAG variant using carbon dioxide — either pure CO2 or argon-CO2 blends — applied to carbon steel and low-alloy steel fabrication.

One common misconception in Indonesia is that CO2 welding is a "low-end" process suited only for thick plate. This is not accurate. The process is used for structural steel, automotive body components, pipe fabrication, and shipbuilding. Its reputation for being rough comes largely from poor parameter settings and inadequate gas coverage, not from any inherent limitation of the process itself. Understanding what the process actually does mechanically is the starting point for getting consistent results. For a broader technical overview of the co2 welding process, the GMAW entry on Wikipedia provides useful background on arc physics and transfer modes.

How the GMAW process works with carbon dioxide shielding gas

The core mechanism is straightforward. A welding power source delivers a continuous DC current. A wire feed welding unit pushes a solid welding electrode wire — typically ER70S-6 at 0.8 mm or 1.0 mm diameter for general steel work — through a liner inside the welding gun. When the wire contacts the base metal, the arc ionizes and generates temperatures above 6,000°C, melting both the wire tip and the surrounding base metal into a shared pool.

The shielding gas — CO2 — flows through the gun nozzle and blankets the weld pool. Its job is to displace oxygen, nitrogen, and hydrogen in the surrounding air. Without this gas shield, those atmospheric elements would dissolve into the molten metal, causing porosity (known locally as keropos), brittleness, and weak fusion.

What makes CO2 behave differently from inert gases like argon is that it is an active gas. At arc temperatures, CO2 dissociates into carbon monoxide and free oxygen. This oxidizing environment affects the metal transfer mode and creates more spatter compared to argon-rich mixtures. However, it also produces deeper penetration into the base metal, which is often desirable for structural joints.

Metal transfer in CO2 welding happens predominantly through two modes depending on the parameter range:

  • Short-circuit transfer (short arc) — the wire tip touches the pool, the arc extinguishes momentarily, the wire melts off, and the arc re-establishes. This repeats at 20–200 times per second. It produces low heat input, which makes it suitable for thin sheet metal (1.5–4 mm), vertical welding, and overhead positions. It is the most common mode in small Indonesian workshops.
  • Globular transfer — occurs at higher voltages. Molten droplets larger than the wire diameter detach irregularly, causing significant spatter. This mode is generally undesirable and is a sign that parameters are mismatched — usually voltage too high relative to wire feed speed.

Spray transfer — the cleanest, lowest-spatter mode — is not achievable with pure CO2. It requires at least 80% argon in the shielding gas mixture. This is one of the main practical reasons to consider argon-CO2 blends for certain applications, which is covered in the next section.

Cross-section diagram of a CO2 welding gun in operation, showing wire feed path, gas nozzle, arc column, weld pool, and CO2 shielding gas coverage over carbon steel base metal

The welding power source in a GMAW setup is typically a constant voltage (CV) machine. Unlike stick welding, which uses constant current, a CV machine maintains a set voltage while the wire feed speed determines the actual amperage. This self-regulating characteristic means that if the arc length shortens, current increases automatically to burn back the wire — keeping the arc stable without manual intervention. This is what makes the process semi-automatic: the welder controls gun movement and position, while the machine regulates the arc.

Setting up parameters: voltage, wire feed, and gas flow for real workshop conditions

Parameter setup is where most welding problems originate. Machines are frequently set by feel or habit rather than by systematic adjustment, which leads to chronic issues with spatter, incomplete fusion, or burn-through on thinner material. The following table covers starting-point parameters for common workshop scenarios using solid wire with pure CO2 shielding gas.

Base metal thickness Wire diameter Voltage (V) Wire feed speed (m/min) CO2 flow rate (L/min)
1.5 – 2.5 mm 0.8 mm 16 – 18 V 3.5 – 5.0 8 – 12
3 – 6 mm 0.9 – 1.0 mm 18 – 22 V 5.0 – 8.0 12 – 15
6 – 12 mm 1.0 – 1.2 mm 22 – 26 V 7.0 – 11.0 15 – 18
12 mm and above 1.2 mm 24 – 28 V 9.0 – 14.0 15 – 20

These are starting points, not fixed values. Actual settings vary with joint geometry, welding position, wire brand, machine calibration, and ambient conditions. The correct approach is to run a test bead on scrap material, assess bead profile and spatter level, then adjust incrementally — one variable at a time.

Voltage and wire feed speed relationship: Voltage controls arc length. Wire feed speed (WFS) controls amperage and deposition rate. The two must be balanced. Increasing WFS without raising voltage produces a stubby, spattery arc. Raising voltage without increasing WFS creates an excessively long arc and risk of undercut.

Gas flow rate: More is not always better. Excessive flow above 20 L/min can create turbulence at the nozzle, pulling in ambient air and causing porosity. In outdoor or semi-outdoor environments — common at Indonesian construction sites and fabrication yards — a physical windshield around the work area is essential. Even moderate wind of 1–2 m/s is enough to strip CO2 coverage from the weld pool.

Contact tip-to-work distance (CTWD): Maintain 10–15 mm for most applications. Longer stick-out increases resistance in the wire, effectively raising heat input without changing the machine setting. Inconsistent CTWD is one of the most overlooked causes of erratic arc behavior in hand welding.

CO2 vs argon-CO2 mixed gas: when to use which

Pure CO2 and argon-CO2 mixed gas (typically 75–80% Ar / 20–25% CO2, sometimes written as C25 or ArCO2) are both used in MAG welding of carbon steel, but they behave differently and suit different priorities.

The key differences come down to arc behavior, spatter, penetration profile, and operating cost:

  • Pure CO2 produces deeper, narrower penetration. It operates in short-circuit or globular transfer mode. Spatter is higher, which means more post-weld cleanup and more wire consumed per finished meter of weld. However, CO2 is significantly less expensive than argon-CO2 blends and is more widely available across Indonesia, including in smaller cities where argon supply can be inconsistent.
  • Argon-CO2 mixed gas allows spray transfer at higher current levels, producing a smooth, low-spatter arc. Bead appearance is cleaner, and the process is easier to control, especially on thinner material or in applications where cosmetic quality matters. The penetration profile is shallower and broader compared to pure CO2, which may require joint preparation adjustments on thicker sections.

For most heavy fabrication, structural steel work, and general-purpose carbon steel welding in Indonesian industrial settings, pure CO2 remains the practical default. The cost difference between CO2 and mixed gas is real and meaningful at scale — a fabrication shop running multiple machines continuously will notice the difference in gas consumption costs and logistics.

Argon-CO2 blends become worth the premium when surface finish matters (automotive components, visible structural members), when welding thinner gauge sheet where spatter control is critical, or when the application calls for higher deposition rates achievable through spray transfer.

One point that often causes confusion: pure argon is not suitable for GMAW on carbon steel. Without CO2 or oxygen in the mix, the arc becomes unstable and fusion quality degrades. Argon as a sole shielding gas works for aluminum and other non-ferrous metals but should not be used for steel wire feed welding. This is a common purchasing error when workshops switch gas suppliers without understanding shielding gas compatibility. For more detail on how shielding gas selection affects the GMAW process, the MIG and CO2 welding guide from Lincoln Electric covers transfer modes and gas selection in depth.

Flux core welding (FCAW) deserves a mention here as a related but distinct option. Flux core welding uses a tubular wire filled with flux compounds instead of a solid wire. Some flux core variants use CO2 or argon-CO2 as an external shielding gas (gas-shielded FCAW), while others are "gasless" and rely entirely on the flux for shielding. FCAW generally offers higher deposition rates than solid wire GMAW and is more tolerant of surface contamination, making it a practical choice for site welding on heavy steel structures where cleaning is difficult. However, it costs more per kilogram of wire and requires more attention to slag removal.

Common problems in CO2 welding and how to solve them

Most recurring quality issues in CO2 welding trace back to a small set of causes. Knowing which symptom points to which cause saves significant diagnostic time on the shop floor.

Excessive spatter

Spatter is the most frequently complained-about issue in las CO2 setups. The causes are usually one of three: voltage too low relative to wire feed speed (producing a harsh, explosive short-circuit arc), voltage too high (producing globular transfer), or a contaminated or worn contact tip causing irregular current delivery. Start by checking the voltage-to-WFS ratio for the material thickness, then inspect the contact tip. Applying anti-spatter spray to the nozzle and workpiece reduces adhesion but does not address the root cause.

Porosity (keropos)

Porosity — small voids visible on the weld surface or in cross-section — is almost always related to shielding gas failure or base metal contamination. Specific causes include:

  • Gas flow rate too low or too high (turbulence)
  • Wind or air movement disrupting the gas shield
  • CO2 regulator or heater malfunction — in Indonesia's climate, a frozen regulator is less common than a faulty or aging heater element that fails to properly warm the gas before it exits the cylinder, reducing stable flow
  • Near-empty gas cylinder where liquid CO2 may partially flow through instead of consistent gas
  • Oil, rust, moisture, paint, or galvanizing on the base metal surface
  • Damaged or kinked gas hose with air ingress

Systematically check each of these before assuming the issue is technique-related.

Burn-through on thin material

Thin sheet (below 2.5 mm) is particularly susceptible to burn-through when parameters are set for thicker stock. Reduce voltage and wire feed speed, shorten arc time by increasing travel speed, and consider using 0.8 mm wire instead of 1.0 mm. Stitch welding — short runs with pauses to allow heat to dissipate — is a standard technique for thin gauge fabrication. Proper fit-up with minimal gap is also essential; a 1 mm gap in thin sheet can be the difference between a sound weld and a hole.

Inconsistent arc or arc interruption

If the arc keeps cutting out or behaving erratically, check the wire feed path: the liner inside the cable assembly accumulates metal dust and debris over time, increasing friction and causing irregular wire delivery. Liners should be cleaned or replaced periodically. Also check the drive roll pressure — too tight deforms the wire and creates feeding resistance; too loose causes slippage. Contact tips wear and develop an oval bore, which allows the wire to wander and arc position to shift.

Lack of fusion

Fusion failure — where the weld metal sits on top of the base metal rather than integrating with it — occurs when heat input is insufficient or travel speed is too fast. With CO2 welding on thicker sections, the deeper penetration profile helps, but it cannot compensate for incorrect technique on joint preparation. Ensure the joint is clean, the bevel angle is appropriate, and the gun angle (typically 10–15° drag angle) directs arc energy into the joint root.

Industrial applications driving demand in Indonesia

CO2 welding is not a niche process in Indonesia — it is the foundational joining method across a range of industries that form the backbone of the country's industrial output. Understanding where the process is applied helps clarify why setup quality and equipment selection matter beyond small workshop settings.

Structural steel fabrication — construction of industrial buildings, bridges, infrastructure, and the ongoing development associated with large-scale projects across the archipelago all depend on carbon steel fabrication. Semi-automatic welding with CO2 or argon-CO2 mixed gas is the standard method for beam-to-column connections, bracket fabrication, and secondary structural members. Welding standards for structural steel work, including joint qualification and inspection requirements, are addressed under frameworks such as those published by the welding standards and processes guidelines from the American Welding Society, which serve as reference documents in many Indonesian engineering projects.

Shipbuilding and marine fabrication — Indonesia's shipbuilding sector, particularly in Batam, Surabaya, and Makassar, relies heavily on GMAW for hull plating, bulkhead fabrication, and deck structure assembly. The combination of high deposition rates, adaptability to various positions, and suitability for classification-grade carbon steel makes CO2 welding the workhorse process in these yards.

Automotive and manufacturing components — automotive sub-assembly production and general manufacturing of machinery, agricultural equipment, and consumer goods all use wire feed welding on carbon steel frames and components. In higher-volume production environments, robotic GMAW systems using either pure CO2 or mixed gas are increasingly common as manufacturers address the ongoing shortage of skilled welders.

Pipeline and pressure vessel fabrication — while root passes on critical pipe joints often use TIG welding for quality control reasons, fill and cap passes on carbon steel piping are routinely completed with CO2 welding processes, particularly in lower-pressure utility piping and structural pipe applications.

The Indonesian welding materials market was valued at approximately USD 441 million in 2025, with projections reaching around USD 561 million by 2030, according to industry data from MarketsandMarkets. Arc welding equipment represents a substantial share of this market, with growth driven by infrastructure spending, downstream nickel processing investment, and the ongoing expansion of manufacturing capacity. Automated and robotic welding is growing as a share of this market, particularly among larger manufacturers, though semi-automatic CO2 welding remains dominant in smaller fabrication operations across the country.

The trend toward inverter-based welding machines is also relevant here. Modern inverter welding power sources are significantly lighter and more energy-efficient than transformer-based machines, and they offer finer parameter control — both of which benefit CO2 welding quality, particularly for smaller workshops where generator power or inconsistent grid supply can affect arc stability.

Frequently asked questions

Can CO2 welding be used on stainless steel or aluminum?

No. Pure CO2 and argon-CO2 blends are not suitable for stainless steel or aluminum. Stainless steel requires a tri-mix shielding gas (typically helium, argon, and CO2 or oxygen in precise proportions) to avoid carbon contamination of the weld. Aluminum requires pure argon as the shielding gas and a different wire alloy. Using CO2 on these materials will produce defective, structurally unsound welds. CO2 welding processes — both solid wire and gas-shielded flux core — are specific to carbon steel and low-alloy steel applications.

What is the difference between CO2 welding and stick welding (SMAW)?

Stick welding (shielded metal arc welding, or SMAW) uses a consumable electrode coated in flux. The flux burns during welding to generate its own shielding gas and slag, requiring no external gas supply. CO2 welding feeds a continuous solid wire and uses an external gas cylinder. CO2 welding generally offers higher deposition rates, better suited to production environments, while stick welding is more portable and tolerant of poor surface conditions. For site work in remote locations where CO2 cylinder supply is impractical, stick welding remains a practical alternative.

Why does my CO2 weld have a lot of spatter even after adjusting the machine?

If parameter adjustment does not resolve spatter, check these mechanical factors: worn or oversized contact tip bore, contaminated or kinked wire liner causing irregular feed, poor electrical connection at the work clamp (ground), or base metal with surface contamination such as mill scale, rust, or oil. Each of these produces arc instability that parameters alone cannot correct. Also verify that the polarity is set to DC electrode positive (DCEP/reverse polarity), which is the correct setting for solid wire CO2 welding. Incorrect polarity produces heavy spatter and poor penetration.

Is CO2 welding the same as MIG welding?

In everyday workshop language, yes — in precise technical terms, no. MIG (metal inert gas welding) refers strictly to processes using an inert shielding gas like argon. CO2 welding uses an active gas and is technically MAG (metal active gas welding). Both fall under the broader GMAW category. In Indonesia and much of Southeast Asia, "MIG welding" is commonly used to describe both, and most welding machine specifications labeled "MIG" support CO2 and argon-CO2 mixed gas operation. The practical implication is that checking the gas compatibility of a machine before purchase matters more than the label on the front panel.

How often should consumables like contact tips and liners be replaced?

Contact tips should be inspected regularly and replaced when the bore becomes visibly enlarged or oval-shaped, which typically occurs after several hours of continuous welding depending on current level and wire diameter. Running with a worn tip is one of the most common causes of erratic arc behavior. Wire liners should be replaced when they show visible kinking, internal clogging from metal dust, or when feed resistance increases noticeably. In high-output production settings, some workshops establish fixed replacement intervals rather than waiting for problems to appear, as unplanned downtime from consumable failure is more costly than scheduled maintenance.

Key words:

Previous: